High viscosity "coatings" act like cold honey; therefore, the lacquer will not "atomize" into small particles and flow out to a level smooth surface before it dries.

Local Companies

Merida Meridian, Inc.
(617) 464-5400
643 Summer Street
Boston, MA
Pann Home Services
(617)8642625
207 Prospect Street
Cambridge, MA
Sullivan Brothers Renovations
781 910-1800
500 Revere Beach Blvrd
Revere, MA
Boston Reno llc
617-641-9111
79 Union st.
Newton, MA
Boston Reno llc
617-641-9111
79 Union st.
Newton, MA
Burns Home Improvements
617-939-7645
59 Main Street
Quincy, MA
Custom Homes
781-850-5266
58 Newcomb Rd
Stoneham, MA
Freeman Decorating Company
(781) 380-7550
1515 Washington Street
Braintree, MA
Dembro Designs and Home Remodeling
781 696-7776
267 Tremont Street
Braintree, MA
Roger P. Toran ... Design~Build
781-444-5966
57 Mary Chilton Road
Needham, MA

provided by: 

Q: We have a small cabinet shop in the Northeastern part of the United States. Every fall my finisher has problems with our precatalyzed lacquer. It will not "flow" out smooth before it dries. It feels rough to the touch, and customers have been complaining about our finish. What has he been doing wrong?

P.S. He has been making the finish "run" and "sag" a lot lately.

A: Generally, this problem relates to cold material temperatures. It is possible that you may be experiencing night time temperatures between 40 to 50 F this time of year, since you are located in the far Northeast. Many shops do not leave the heat turned up at nighttime or store their coating material in a location where the coating material temperatures can easily drop to 60 F or less. A 10-degree drop from 72 F will increase your coating's viscosity up to as much as 30 percent.

High viscosity "coatings" act like cold honey; therefore, the lacquer will not "atomize" into small particles and flow out to a level smooth surface before it dries. Other problems can cause this defect; however, this roughness or "orange peel" effect — plus experiencing problems with runs and sags — indicate that this issue is related to cold material temperatures.

You could try bringing the coating material temperature up by placing the pails of coating in a safe heated area the night before use. This should solve your problem. It is always important to ensure finishing materials are above 72 F before using.

Ed. note: Phil Stevenson is the founder of the American Wood Finishing Institute (AWFI) in Vineland, N.J.

author: By Phil Stevenson


Featured Local Company

Merida Meridian, Inc.

(617) 464-5400
643 Summer Street
Boston, MA

Related Local Events
Lumber & Building Material Expo
Dates: 2/3/2010 - 2/5/2010
Location: Seaport World Trade Center, Boston
Boston, MA
View Details

Suburban Boston Spring Home Show
Dates: 2/12/2010 - 2/14/2010
Location: Shriners Auditorium
Wilmington, MA
View Details

Build Boston 2009
Dates: 11/18/2009 - 11/20/2009
Location: Seaport World Trade Center
Boston, ME
View Details

AEBE
Dates: 11/18/2009 - 11/20/2009
Location: Hynes Convention Center
Boston, MA
View Details

Greenbuild - International Conference and Expo for Green Building Industry 2009
Dates: 11/11/2009 - 11/13/2009
Location: Boston Convention & Exhibition Center
Boston, MA
View Details